Search This Blog

Showing posts with label 63/37 Solder. Show all posts
Showing posts with label 63/37 Solder. Show all posts

Saturday, July 2, 2016

B.I.C SMD SMT Solder Paste 63-37 (Sn/Pb) Solder Paste No-Clean

B.I.C 63/37 No Clean Solder Paste 





B.I.C SMD Paste series are middle activity resin based no clean type solder paste. Especially designed no clean flux for soldering where residues are indecomposable.

Monday, June 20, 2016

B.I.C 63/37 No Clean Flux Core Solder Wire

63/37 No Clean Wire
No-Clean cored wires was developed to eliminate the use of solvents for post-solder cleaning of circuit board assemblies in electronic industry. The No-Clean flux used in the wire core is completely halide-free. It provides excellent solderabilty and high reliability. The flux residues requires no-cleaning due to physio-chemical characteristics of the core flux.

Available in 16, 18, 20, 22 SWG (Wire Diameter/Thickness)
Made to Order in 24 SWG and 26 SWG

Melting Temp. 
SOLIDUS: 183*c
LIQUIDUS: 183*c

Usage:

1. Application which does not require product to sustain high temperature.
2. Application which require Premium QUALITY shine in Solder joints.
3. For PCB Soldering and Product adhering EU Standards.
4. Shrink pack Reels for best appeal and Protection of the product from oxidation.
5. Available in Different Flux Core Ratios. (1.2 % to 2.4%)
6. Less Smoke and subtle smell than any other brand.

Specs:

1. High Solder Flow, Non-Corrosive, Non-Conductive
2. Works @ Fast Soldering. Helps to achieve high Efficiency.
3. Less smoke compared to other brands.
4. Resin Activated Wire Solder.

Application:
For Electronic GRADE Application Use Only.
- One should bear that Flow is always less compared to Rosin Cored Wire.
- Flux does not required to be cleaned (exceptions are there)

More Details:

Recommended Iron Wattage.
10 Watt for 22 SWG
25 watt for 20 SWG
35 Watt for 18 SWG
65 Watt for 16 SWG

About No-Clean Flux Wire:

Soldering requires flux to removes oxides and to promote wetting. Rosin (made from tree sap) is one flux material that has long been popular, and comes in various strengths- RMA (Rosin Mildly Activated) or RA (Rosin Activated). 

We ensure that you can leave the flux on the board under fairly benign conditions and experience bears that out (it only becomes active = corrosive) at elevated temperatures, however most manufacturers will clean the board for cosmetic reasons and to allow inspection. Cleaning often involves the use of petroleum solvents (PCB Cleaning Solvents)- for example by vapor degreasing or just scrubbing.

No clean fluxes allegedly don't need to be cleaned and can be left on the board, however many of have had problems with no-clean processes having relatively conductive residue. The residue is ironically extremely hard to remove, much more difficult than the two above-mentioned processes, more like 'can't clean'. Think twice about this kind of flux if you're thinking of sensitive analog boards that have high impedance. Even circuits you may not think of as being analog such as RTCC chips with an external crystal may be affected.

Safest for sensitive boards is rosin flux followed by a thorough cleaning process(using PCB Cleaning Solvents).

No clean flux often has enough "low" resistance that it might influence sensitive circuits, so in case you can withstand with a few hundreds of megohms resistance between anything, leave it on. If that is too low, clean it up.

Also Visit our other Solder Wire/Sticks range:
 Sharp Wire Solder (No Clean /Urea Flux Wire),         Lumax Wire Solder,        60/40 Standard Wire,                
  60/40 Premium Wire,              60/40 No Clean Wire Solder,          63/37 Quality Wire,                                                                            



Best Regards,
B.I.C Solder Team

BAJAJ INSULATION CO. MANUFACTURES SOLDER WIRE, SOLDER STICKS, SOLDER FLUXES, PCB CLEANING SOLVENTS, DIP SOLDERING MACHINES, TIN-COPPER WIRE, TIN-ZINC WIRE AND ALLIED CHEMICALS IN DELHI.

Sunday, June 19, 2016

B.I.C 63/37 Rosin Core WIRE SOLDER and Sticks/Rods




RA Type rosin cored wire is available in all type of solder alloys, different sizes and varying core percentages. It is used for Soldering any kind of electronic assemblies. It provides instant wetting and excellent capillary action which results in less rejections and few touch-ups.
This type of wire is suitable for soldering oxidized and difficult to solder metals. The flux residue left after soldering is considered to be non-conductive non-hygroscopic and can be removed by, solvent cleaning process.

Available in 10, 12, 14, 16, 18, 20, 22 SWG (Wire Diameter/Thickness)
                                         Custom Made Order in 24 SWG and 26 SWG
Melting Temp.
SOLIDUS: 183*c
LIQUIDUS: 183*c

Specific Gravity: 8.4
Color: Silver white alloy wire
Boiling Point: Hazardous concentration of lead are given off at temperature above 450*C

Usage:

1. Application which require product to sustain high temperature.
2. Application which require Premium QUALITY shine in Solder joints.
5. Shrink pack Reels for best appeal and Protection of the product.
6. Available in Rosin Core and No Clean Core.
7. Available in Different Flux Core Ratios. (2 % to 2.8%)
8. ABOVE QUALITY IS IN HIGH QUALITY ROSIN CORE FLUX.
9. Less Smoke than any other brand.

Specs:

1. High Solder Flow, Non-Corrosive, 
2. Works @ Fast Soldering. Helps to achieve high Efficiency.
3. Less smoke compared to other brands.
4. Activated Wire Solder.

Application:
For Electronic GRADE Application Use Only.
For Wave Soldering.

More Details:

Recommended Iron Wattage.
10 Watt for 22 SWG
25 watt for 20 SWG
35 Watt for 18 SWG
65 Watt for 16 SWG

B.I.C PURE 63/37 RATIO STICKS

 

Details:

Our technologically advance Nitrogen blast furnace process coupled with dross reducing treatment while producing solder bars ensure less oxide solder rods to ensure min. dross formation at your end to save hugely on your production cost and efficiency.

1. PURE Oxide-Free Stick/Rod which means min. Dross bars. 

    One cannot ascertain Dross in Stick from outside. Regular bars contain 30% Dross inside it. Purchasing Cheap Rod which is not Oxide free means paying for Dross at the price of Solder.

2. Strong Physical Joints.
4. Require at least 230*C to melt in Dip Machine
5. Save on your Solder cost by upto 50%. Refer this link Anti-DrossFormulation








Also Visit our Premium Solder Wire/Sticks range:

 Sharp Wire Solder (No Clean /Urea Flux Wire),              Lumax Wire Solder,              60/40 Standard Wire,                
  60/40 Premium Wire,              60/40 No Clean Wire Solder,                            63/37 No Clean Wire.

Best Regards,
B.I.C Solder Team

BAJAJ INSULATION CO. MANUFACTURES SOLDER WIRE, SOLDER STICKS, SOLDER FLUXES, PCB CLEANING SOLVENTS, DIP SOLDERING MACHINES, TIN-COPPER WIRE, TIN-ZINC WIRE AND ALLIED CHEMICALS IN DELHI.